Product Overview
CK0.07 Low-Calcium Lead Alloy Foil is silver-modified lead-calcium alloy foil, calcium content 0.05–0.09% with trace silver as modifier, extra soft annealed temper, fully compliant with GOST CK0.07, JIS H4301 and IEC60404 standards. Compared with PbCa0.07, trace silver further improves alloy stability and anti-fatigue property, suitable for high requirement long-life composite sealing structures, especially for CIS and Russian engineering projects.
Available thickness 0.02–100μm, coil width 200–1220mm, single coil length 1000–10000m. Tensile strength 24–32MPa, elongation 25–33%, density 11.29g/cm³. Main application: high stability composite sealing laminate, chemical anti-corrosion lining, static load gasket materials and light radiation shielding composite parts.
Surface choices: matte rolled surface, anti-oxidation passivation coating and PET composite film. Custom protective packaging. MOQ 5 ton, payment T/T or L/C sight, lead time 7–15 working days, GOST format MTC certificate available.
Chemical & Mechanical Property Snapshot
Detailed Technical Specifications
Product Comparison Table
App Market
Reliable Steel Coil Solutions For Diverse Industrial Applications
Product Packaging
Secure Export Packaging For Safe Handling And Delivery
FAQs
CK0.07 is GOST standard lead-calcium alloy with trace silver modifier, widely used in Russian and CIS market for sealing composite materials.
CK0.07 contains trace silver modifier for better anti-fatigue and long-term stability.
Yes, we can provide MTC certificate complying with GOST standard.
Extra soft annealed temper, good bending and composite performance.
High stability composite sealing gasket, chemical corrosion resistant lining for long service life.